| UNS • Canonical Grade | Subfamily | Standard Identifiers | Conductivity (% IACS) | Yield & Context | Status | Actions |
|---|---|---|---|---|---|---|
| 1050 Aluminum1050A | Wrought Aluminum Alloys | AA: 1050UNS: A91050EN: EN AW-1050A | — | ≥ 20 MPaMINIMUM · O Temper · Sheet · 0.2mm to 6.0mm | VERIFIED | |
| 3103 AluminumEN AW-3103 | Wrought Aluminum Alloys | AA: 3103UNS: A93103EN: EN AW-3103 | — | ≥ 115 MPaMINIMUM · H14 Temper · Sheet · 0.2mm to 6.0mm | VERIFIED | |
| 5005 AluminumEN AW-5005 | Wrought Aluminum Alloys | AA: 5005UNS: A95005EN: EN AW-5005 | — | ≥ 110 MPaMINIMUM · H34 Temper · Sheet · 0.2mm to 12.5mm | VERIFIED | |
| 5083 AluminumEN AW-5083 | Wrought Aluminum Alloys | AA: 5083UNS: A95083EN: EN AW-5083 | — | ≥ 125 MPaMINIMUM · O / H111 Temper · Sheet · 0.2mm to 6.3mm | VERIFIED | |
| 5251 AluminumEN AW-5251 | Wrought Aluminum Alloys | AA: 5251UNS: A95251EN: EN AW-5251 | — | ≥ 60 MPaMINIMUM · O Temper · Sheet & Plate · 0.2mm to 50.0mm | VERIFIED | |
| 5454 AluminumEN AW-5454 | Wrought Aluminum Alloys | AA: 5454UNS: A95454EN: EN AW-5454 | — | ≥ 85 MPaMINIMUM · O / H111 Temper · Sheet · 0.2mm to 6.0mm | VERIFIED | |
| 5754 AluminumEN AW-5754 | Wrought Aluminum Alloys | AA: 5754UNS: A95754EN: EN AW-5754 | — | ≥ 80 MPaMINIMUM · H111 Temper · Sheet · 0.2mm to 6.0mm | VERIFIED | |
| 6005A AluminumEN AW-6005A | Wrought Aluminum Alloys | AA: 6005AUNS: A96005EN: EN AW-6005A | — | ≥ 225 MPaMINIMUM · T6 Temper · Extrusions · up to 5mm | VERIFIED | |
| 6026 AluminumEN AW-6026 | Wrought Aluminum Alloys | AA: 6026UNS: A96026EN: EN AW-6026 | — | ≥ 360 MPaMINIMUM · T9 Temper · Extruded and Drawn Bar | VERIFIED | |
| 6060 AluminumEN AW-6060 | Wrought Aluminum Alloys | AA: 6060UNS: A96060EN: EN AW-6060 | — | ≥ 120 MPaMINIMUM · T5 Temper · Extrusions · Up to 150mm Dia., 15mm WT tube, 5mm WT profiles | VERIFIED | |
| 6082 AluminumEN AW-6082 | Wrought Aluminum Alloys | AA: 6082UNS: A96082EN: EN AW-6082 | — | ≤ 85 MPaMAXIMUM · O Temper · Sheet · 0.4mm to 6.0mm | VERIFIED | |
| 6101 AluminumEN AW-6101 | Wrought Aluminum Alloys | AA: 6101UNS: A96101EN: EN AW-6101 | — | ≥ 170 MPaMINIMUM · T6 Temper · Extruded Bar · up to 150mm | VERIFIED | |
| 6106 AluminumEN AW-6106 | Wrought Aluminum Alloys | AA: 6106UNS: A96106EN: EN AW-6106 | — | ≥ 200 MPaMINIMUM · T6 Temper · Extruded Profiles · up to 10mm WT | VERIFIED | |
| 6262 AluminumEN AW-6262 | Wrought Aluminum Alloys | AA: 6262UNS: A96262EN: EN AW-6262 | — | ≥ 240 MPaMINIMUM · T6 Temper · Extrusions · up to 200mm Dia | VERIFIED | |
| 1100 AluminumAA 1100 | Wrought Aluminum Alloys | AA: 1100UNS: A91100ISO: Al99.0Cu | 59 % IACSTYPICAL · O Temper | 34 MPaTYPICAL · O Temper · Drawn Tube | VERIFIED | |
| 2011 AluminumAA 2011 | Wrought Aluminum Alloys | AA: 2011UNS: A92011ISO: AlCu6BiPb | 39 % IACSTYPICAL · T3 Temper | 296 MPaTYPICAL · T3 Temper · Cold Finished Rod & Bar | VERIFIED | |
| 2014 AluminumAA 2014 | Wrought Aluminum Alloys | AA: 2014UNS: A92014ISO: AlCu4SiMg | 50 % IACSTYPICAL · O Temper | 97 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 2017 AluminumAA 2017 | Wrought Aluminum Alloys | AA: 2017UNS: A92017ISO: AlCu4MgSi | 50 % IACSTYPICAL · O Temper | 70 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 2024 AluminumAA 2024 | Wrought Aluminum Alloys | AA: 2024UNS: A92024ISO: AlCu4Mg1 | 50 % IACSTYPICAL · O Temper | 76 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 3003 AluminumAA 3003 | Wrought Aluminum Alloys | AA: 3003UNS: A93003ISO: AlMn1Cu | 50 % IACSTYPICAL · O Temper | 41 MPaTYPICAL · O Temper · Drawn Tube | VERIFIED | |
| 5052 AluminumAA 5052 | Wrought Aluminum Alloys | AA: 5052UNS: A95052ISO: AlMg2.5 | 35 % IACSTYPICAL | 90 MPaTYPICAL · O Temper · Drawn Tube | VERIFIED | |
| 6061 AluminumAA 6061 | Wrought Aluminum Alloys | AA: 6061UNS: A96061ISO: AlMg1SiCu | 47 % IACSTYPICAL · O Temper | 55 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 6063 AluminumAA 6063 | Wrought Aluminum Alloys | AA: 6063UNS: A96063ISO: AlMg0.7Si | 58 % IACSTYPICAL · O Temper | 48 MPaTYPICAL · O Temper · Drawn Tube | VERIFIED | |
| 7050 AluminumAA 7050 | Wrought Aluminum Alloys | AA: 7050UNS: A97050ISO: AlZn6CuMgZr | 39.5 % IACSTYPICAL · T76, T76511 Temper | 469 MPaTYPICAL · T7451 Temper · Plate · LONGITUDINAL | VERIFIED | |
| 7075 AluminumAA 7075 | Wrought Aluminum Alloys | AA: 7075UNS: A97075ISO: AlZn5.5MgCu | 45 % IACSTYPICAL · O Temper | 103 MPaTYPICAL · O Temper · Cold Finished Rod & Bar | VERIFIED | |
| 7175 AluminumAA 7175 | Wrought Aluminum Alloys | AA: 7175UNS: A97175ISO: AlZn5.5MgCu(B) | 33 % IACSTYPICAL · T66 Temper | 510 MPaTYPICAL · T66 Temper · Forgings | VERIFIED | |
| 7475 AluminumAA 7475 | Wrought Aluminum Alloys | AA: 7475UNS: A97475ISO: AlZn5.5MgCu(A) | 36 % IACSTYPICAL · T651 Temper | 510 MPaTYPICAL · T651 Temper · Sheet & Plate | VERIFIED |
Verified Aluminum Alloys Comparison Pairs (4)
Open Compare Engine →Selection between general-purpose weldable aluminum and ultra-high-strength aerospace zinc-alloyed aluminum.
Structural load capacity versus architectural extrusion complexity and anodized cosmetic surface finish.
Sheet metal bending radii and marine salt-spray endurance vs CNC machining rigidity and structural strength.
Fatigue crack growth resistance and fracture toughness (tension applications) vs peak static compressive and tensile yield strength.
How to Weld Aluminium to Aluminium: TIG, MIG, Filler Metals & Alloy Guide →
Master the physical metallurgy of joining aluminium alloys. Learn how to overcome the refractory 2,072°C Al₂O₃ oxide layer, calibrate AC balance on TIG inverters, configure MIG spool guns, choose between ER4043 and ER5356 filler wires, and manage heat-affected zone (HAZ) softening across 6061-T6, 6063, 5052, and casting alloys.