Verified Production Database

Materials Directory

Explore 173 verified stainless steel, steel, aluminum, copper, cast iron, silver, and rubber & elastomers alloys. Review condition-specific properties, composition limits, and authoritative standard references.

Filter Material Subfamily:
173 Material Records Qualified
Sort By:
Scroll horizontally for full specifications
Designation • Canonical GradeSubfamilyStandard IdentifiersConductivity (% IACS)Yield & ContextDensityStatusActions
1050 Aluminum1050AWrought Aluminum Alloys
AA: 1050UNS: A91050EN: EN AW-1050A
—≥ 20 MPaMINIMUM · O Temper · Sheet · 0.2mm to 6.0mm2.71 g/cm³TYPICALVERIFIED
Specs|
1100 AluminumAA 1100Wrought Aluminum Alloys
AA: 1100UNS: A91100ISO: Al99.0Cu
59 % IACSTYPICAL · O Temper34 MPaTYPICAL · O Temper · Drawn Tube2.71 g/cm³TYPICALVERIFIED
Specs|
17-4 PH (630) Stainless SteelPrecipitation Hardening
COMMERCIAL: 17-4 PHTYPE: 630UNS: S17400
—1275.5 MPaTYPICAL · H900 · Bar · LONGITUDINAL · Typical longitudinal bar properties; section dimensions and test temperature not stated in this table. Not minimum requirements.7.78 g/cm³TYPICAL · Condition A · Source temperature not specified. Metric density retained independently; rounded imperial equivalents are not used.VERIFIED
Specs|
201 Stainless SteelAustenitic
TYPE: 201SPECIFICATION: 201 Stainless Steel Engineering Datasheet
—≥ 310 MPaMINIMUM · Annealed · Sheet and Strip7.81 g/cm³TYPICALVERIFIED
Specs|
2011 AluminumAA 2011Wrought Aluminum Alloys
AA: 2011UNS: A92011ISO: AlCu6BiPb
39 % IACSTYPICAL · T3 Temper296 MPaTYPICAL · T3 Temper · Cold Finished Rod & Bar2.82 g/cm³TYPICALVERIFIED
Specs|
2014 AluminumAA 2014Wrought Aluminum Alloys
AA: 2014UNS: A92014ISO: AlCu4SiMg
50 % IACSTYPICAL · O Temper97 MPaTYPICAL · O Temper · Cold Finished Rod & Bar2.8 g/cm³TYPICALVERIFIED
Specs|
2017 AluminumAA 2017Wrought Aluminum Alloys
AA: 2017UNS: A92017ISO: AlCu4MgSi
50 % IACSTYPICAL · O Temper70 MPaTYPICAL · O Temper · Cold Finished Rod & Bar2.79 g/cm³TYPICALVERIFIED
Specs|
202 Stainless SteelAustenitic
TYPE: 202SPECIFICATION: 202 Stainless Steel Engineering Datasheet
—≥ 310 MPaMINIMUM · Annealed · Sheet and Strip7.8 g/cm³TYPICALVERIFIED
Specs|
2024 AluminumAA 2024Wrought Aluminum Alloys
AA: 2024UNS: A92024ISO: AlCu4Mg1
50 % IACSTYPICAL · O Temper76 MPaTYPICAL · O Temper · Cold Finished Rod & Bar2.77 g/cm³TYPICALVERIFIED
Specs|
3003 AluminumAA 3003Wrought Aluminum Alloys
AA: 3003UNS: A93003ISO: AlMn1Cu
50 % IACSTYPICAL · O Temper41 MPaTYPICAL · O Temper · Drawn Tube2.73 g/cm³TYPICALVERIFIED
Specs|
301 Stainless SteelAustenitic
TYPE: 301SPECIFICATION: 301 Stainless Steel Engineering Datasheet
—≥ 276 MPaMINIMUM · Annealed · Sheet and Strip7.88 g/cm³TYPICALVERIFIED
Specs|
302 Stainless SteelAustenitic
TYPE: 302SPECIFICATION: 302 Stainless Steel Engineering Datasheet
—≥ 205 MPaMINIMUM · Annealed · Sheet and Strip7.9 g/cm³TYPICALVERIFIED
Specs|
303 Stainless SteelAustenitic
TYPE: 303SPECIFICATION: 303 Stainless Steel Engineering Datasheet
—≥ 205 MPaMINIMUM · Cold Finished Annealed Bar · Bar7.9 g/cm³TYPICALVERIFIED
Specs|
304 Stainless SteelAustenitic
TYPE: 304UNS: S30400SPECIFICATION: 304 Stainless Steel Engineering Datasheet
—≥ 206.8 MPaMINIMUM · ASTM requirements (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee.7.9 g/cm³TYPICAL · Published metric value; no test temperature stated.VERIFIED
Specs|
304L Stainless SteelAustenitic
TYPE: 304LUNS: S30403SPECIFICATION: 304L Stainless Steel Engineering Datasheet
—≥ 172.4 MPaMINIMUM · ASTM requirements (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee.7.9 g/cm³TYPICAL · Published metric value; no test temperature stated.VERIFIED
Specs|
305 Stainless SteelAustenitic
TYPE: 305SPECIFICATION: 305 Stainless Steel Engineering Datasheet
—≥ 170 MPaMINIMUM · Annealed · Sheet and Strip7.9 g/cm³TYPICALVERIFIED
Specs|
309 Stainless SteelAustenitic
TYPE: 309SPECIFICATION: 309 Stainless Steel Engineering Datasheet
—≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip7.9 g/cm³TYPICALVERIFIED
Specs|
310 Stainless SteelAustenitic
TYPE: 310SPECIFICATION: 310 Stainless Steel Engineering Datasheet
—≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip7.9 g/cm³TYPICALVERIFIED
Specs|
3103 AluminumEN AW-3103Wrought Aluminum Alloys
AA: 3103UNS: A93103EN: EN AW-3103
—≥ 115 MPaMINIMUM · H14 Temper · Sheet · 0.2mm to 6.0mm2.73 g/cm³TYPICALVERIFIED
Specs|
316 Stainless SteelAustenitic
TYPE: 316UNS: S31600SPECIFICATION: 316 Stainless Steel Engineering Datasheet
—≥ 206.8 MPaMINIMUM · ASTM requirements at room temperature (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. Source specifies room temperature without a numeric temperature.7.9 g/cm³TYPICAL · Published metric value; no test temperature stated.VERIFIED
Specs|
316L Stainless SteelAustenitic
TYPE: 316LUNS: S31603SPECIFICATION: 316L Stainless Steel Engineering Datasheet
—≥ 172.4 MPaMINIMUM · ASTM requirements at room temperature (producer sheet) · Plate · Separate ASTM grade column in producer datasheet; heat treatment and thickness applicability not stated for these requirements. Typical 0.375-inch plate column is not reused as a guarantee. Source specifies room temperature without a numeric temperature.7.9 g/cm³TYPICAL · Published metric value; no test temperature stated.VERIFIED
Specs|
321 Stainless SteelAustenitic
TYPE: 321SPECIFICATION: 321 Stainless Steel Engineering Datasheet
—≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip7.9 g/cm³TYPICALVERIFIED
Specs|
347 Stainless SteelAustenitic
TYPE: 347SPECIFICATION: 347 Stainless Steel Engineering Datasheet
—≥ 205 MPaMINIMUM · Annealed · Plate, Sheet and Strip7.96 g/cm³TYPICALVERIFIED
Specs|
409 Stainless SteelFerritic
TYPE: 409UNS: S40920SPECIFICATION: 409 Stainless Steel Engineering Datasheet
—≥ 170 MPaMINIMUM · Annealed · Sheet and Strip7.7 g/cm³TYPICALVERIFIED
Specs|
410 Stainless SteelMartensitic
TYPE: 410SPECIFICATION: 410 Stainless Steel Engineering Datasheet
—≥ 205 MPaMINIMUM · Annealed · Bar and Sheet7.75 g/cm³TYPICALVERIFIED
Specs|
420 Stainless SteelMartensitic
TYPE: 420SPECIFICATION: 420 Stainless Steel Engineering Datasheet
—≥ 345 MPaMINIMUM · Annealed · Bar and Strip7.75 g/cm³TYPICALVERIFIED
Specs|
5005 AluminumEN AW-5005Wrought Aluminum Alloys
AA: 5005UNS: A95005EN: EN AW-5005
—≥ 110 MPaMINIMUM · H34 Temper · Sheet · 0.2mm to 12.5mm2.7 g/cm³TYPICALVERIFIED
Specs|
5052 AluminumAA 5052Wrought Aluminum Alloys
AA: 5052UNS: A95052ISO: AlMg2.5
35 % IACSTYPICAL90 MPaTYPICAL · O Temper · Drawn Tube2.68 g/cm³TYPICALVERIFIED
Specs|
5083 AluminumEN AW-5083Wrought Aluminum Alloys
AA: 5083UNS: A95083EN: EN AW-5083
—≥ 125 MPaMINIMUM · O / H111 Temper · Sheet · 0.2mm to 6.3mm2.65 g/cm³TYPICALVERIFIED
Specs|
5251 AluminumEN AW-5251Wrought Aluminum Alloys
AA: 5251UNS: A95251EN: EN AW-5251
—≥ 60 MPaMINIMUM · O Temper · Sheet & Plate · 0.2mm to 50.0mm2.69 g/cm³TYPICALVERIFIED
Specs|
5454 AluminumEN AW-5454Wrought Aluminum Alloys
AA: 5454UNS: A95454EN: EN AW-5454
—≥ 85 MPaMINIMUM · O / H111 Temper · Sheet · 0.2mm to 6.0mm2.68 g/cm³TYPICALVERIFIED
Specs|
5754 AluminumEN AW-5754Wrought Aluminum Alloys
AA: 5754UNS: A95754EN: EN AW-5754
—≥ 80 MPaMINIMUM · H111 Temper · Sheet · 0.2mm to 6.0mm2.66 g/cm³TYPICALVERIFIED
Specs|
6005A AluminumEN AW-6005AWrought Aluminum Alloys
AA: 6005AUNS: A96005EN: EN AW-6005A
—≥ 225 MPaMINIMUM · T6 Temper · Extrusions · up to 5mm2.7 g/cm³TYPICALVERIFIED
Specs|
6026 AluminumEN AW-6026Wrought Aluminum Alloys
AA: 6026UNS: A96026EN: EN AW-6026
—≥ 360 MPaMINIMUM · T9 Temper · Extruded and Drawn Bar2.72 g/cm³TYPICALVERIFIED
Specs|
6060 AluminumEN AW-6060Wrought Aluminum Alloys
AA: 6060UNS: A96060EN: EN AW-6060
—≥ 120 MPaMINIMUM · T5 Temper · Extrusions · Up to 150mm Dia., 15mm WT tube, 5mm WT profiles2.7 g/cm³TYPICALVERIFIED
Specs|
6061 AluminumAA 6061Wrought Aluminum Alloys
AA: 6061UNS: A96061ISO: AlMg1SiCu
47 % IACSTYPICAL · O Temper55 MPaTYPICAL · O Temper · Cold Finished Rod & Bar2.7 g/cm³TYPICALVERIFIED
Specs|
6063 AluminumAA 6063Wrought Aluminum Alloys
AA: 6063UNS: A96063ISO: AlMg0.7Si
58 % IACSTYPICAL · O Temper48 MPaTYPICAL · O Temper · Drawn Tube2.69 g/cm³TYPICALVERIFIED
Specs|
6082 AluminumEN AW-6082Wrought Aluminum Alloys
AA: 6082UNS: A96082EN: EN AW-6082
—≤ 85 MPaMAXIMUM · O Temper · Sheet · 0.4mm to 6.0mm2.7 g/cm³TYPICALVERIFIED
Specs|
6101 AluminumEN AW-6101Wrought Aluminum Alloys
AA: 6101UNS: A96101EN: EN AW-6101
—≥ 170 MPaMINIMUM · T6 Temper · Extruded Bar · up to 150mm2.7 g/cm³TYPICALVERIFIED
Specs|
6106 AluminumEN AW-6106Wrought Aluminum Alloys
AA: 6106UNS: A96106EN: EN AW-6106
—≥ 200 MPaMINIMUM · T6 Temper · Extruded Profiles · up to 10mm WT2.7 g/cm³TYPICALVERIFIED
Specs|
6262 AluminumEN AW-6262Wrought Aluminum Alloys
AA: 6262UNS: A96262EN: EN AW-6262
—≥ 240 MPaMINIMUM · T6 Temper · Extrusions · up to 200mm Dia2.71 g/cm³TYPICALVERIFIED
Specs|
7050 AluminumAA 7050Wrought Aluminum Alloys
AA: 7050UNS: A97050ISO: AlZn6CuMgZr
39.5 % IACSTYPICAL · T76, T76511 Temper469 MPaTYPICAL · T7451 Temper · Plate · LONGITUDINAL2.83 g/cm³TYPICALVERIFIED
Specs|
7075 AluminumAA 7075Wrought Aluminum Alloys
AA: 7075UNS: A97075ISO: AlZn5.5MgCu
45 % IACSTYPICAL · O Temper103 MPaTYPICAL · O Temper · Cold Finished Rod & Bar2.8 g/cm³TYPICALVERIFIED
Specs|
7175 AluminumAA 7175Wrought Aluminum Alloys
AA: 7175UNS: A97175ISO: AlZn5.5MgCu(B)
33 % IACSTYPICAL · T66 Temper510 MPaTYPICAL · T66 Temper · Forgings2.8 g/cm³TYPICALVERIFIED
Specs|
7475 AluminumAA 7475Wrought Aluminum Alloys
AA: 7475UNS: A97475ISO: AlZn5.5MgCu(A)
36 % IACSTYPICAL · T651 Temper510 MPaTYPICAL · T651 Temper · Sheet & Plate2.8 g/cm³TYPICALVERIFIED
Specs|
ASTM A36 Structural SteelCarbon Steel
ASTM: A36
—≥ 248.2 MPaMINIMUM · Producer-stated plate requirements; heat treatment not stated · Finished plate; excludes coil pending conversion and qualification · 2.54–152 mm · TRANSVERSE · Original imperial producer requirements retained; do not apply to unqualified coil. Test temperature not stated.—VERIFIED
Specs|
ASTM A48 Class 20 Gray Cast IronClass 20 Gray IronGray Cast Iron
ASTM: A48 Class 20UNS: F11401SAE: J431 G2000
——7.1 g/cm³TYPICALVERIFIED
Specs|
ASTM A48 Class 25 Gray Cast IronClass 25 Gray IronGray Cast Iron
ASTM: A48 Class 25UNS: F11701SAE: J431 G2500
——7.15 g/cm³TYPICALVERIFIED
Specs|
ASTM A48 Class 30 Gray Cast IronClass 30 Gray IronGray Cast Iron
ASTM: A48 Class 30UNS: F12101SAE: J431 G3000
——7.2 g/cm³TYPICALVERIFIED
Specs|
ASTM A48 Class 35 Gray Cast IronClass 35 Gray IronGray Cast Iron
ASTM: A48 Class 35UNS: F12401SAE: J431 G3500
——7.2 g/cm³TYPICALVERIFIED
Specs|
ASTM A48 Class 40 Gray Cast IronClass 40 Gray IronGray Cast Iron
ASTM: A48 Class 40UNS: F12801SAE: J431 G4000
——7.25 g/cm³TYPICALVERIFIED
Specs|
ASTM A48 Class 50 Gray Cast IronClass 50 Gray IronGray Cast Iron
ASTM: A48 Class 50UNS: F13501SAE: J431 G5000
——7.3 g/cm³TYPICALVERIFIED
Specs|
ASTM A536 Grade 100-70-03 Ductile Cast IronDuctile Iron 100-70-03Ductile (Nodular) Iron
ASTM: A536 Grade 100-70-03UNS: F34800SAE: J434 D7003
—≥ 483 MPaMINIMUM · Normalized or Q&T · Governing minimum 0.2% offset yield strength per ASTM A536 (70 ksi = 483 MPa).7.15 g/cm³TYPICALVERIFIED
Specs|
ASTM A536 Grade 120-90-02 Ductile Cast IronDuctile Iron 120-90-02Ductile (Nodular) Iron
ASTM: A536 Grade 120-90-02UNS: F36200SAE: J434 D9002
—≥ 621 MPaMINIMUM · Quenched and Tempered · Governing minimum 0.2% offset yield strength per ASTM A536 (90 ksi = 621 MPa).7.15 g/cm³TYPICALVERIFIED
Specs|
ASTM A536 Grade 60-40-18 Ductile Cast IronDuctile Iron 60-40-18Ductile (Nodular) Iron
ASTM: A536 Grade 60-40-18UNS: F32800SAE: J434 D4018
—≥ 276 MPaMINIMUM · Annealed or As-Cast · Governing minimum 0.2% offset yield strength per ASTM A536 (40 ksi = 276 MPa).7.1 g/cm³TYPICALVERIFIED
Specs|
ASTM A536 Grade 65-45-12 Ductile Cast IronDuctile Iron 65-45-12Ductile (Nodular) Iron
ASTM: A536 Grade 65-45-12UNS: F33100SAE: J434 D4512
—≥ 310 MPaMINIMUM · As-Cast · Governing minimum 0.2% offset yield strength per ASTM A536 (45 ksi = 310 MPa).7.1 g/cm³TYPICALVERIFIED
Specs|
ASTM A536 Grade 80-55-06 Ductile Cast IronDuctile Iron 80-55-06Ductile (Nodular) Iron
ASTM: A536 Grade 80-55-06UNS: F33800SAE: J434 D5506
—≥ 379 MPaMINIMUM · As-Cast or Normalized · Governing minimum 0.2% offset yield strength per ASTM A536 (55 ksi = 379 MPa).7.15 g/cm³TYPICALVERIFIED
Specs|
Britannia Silver 958Britannia SilverAlloyed Silver
UK-HALLMARK: 958ISO: Ag958DIN: Ag958
92 % IACSTYPICAL · 20 °C≥ 80 MPaTYPICAL · Annealed (Soft) · Strip, Sheet, Wire10.4 g/cm³TYPICAL · 20 °CVERIFIED
Specs|
Butyl Rubber (IIR)Isobutylene Isoprene RubberWeathering & Chemical Resistant Elastomers
ASTM: IIRISO: IIRASTM-D2000: Type BA
———VERIFIED
Specs|
C10100 Oxygen-Free Electronic (OFE) CopperOxygen-Free ElectronicPure Copper
UNS: C10100COMMERCIAL: Oxygen-Free Electronic CopperCDA: Alloy 101
101 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 101.0 % IACS at 68°F (20°C)248.2 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C10200 Oxygen-Free (OF) CopperOxygen-FreePure Copper
UNS: C10200COMMERCIAL: Oxygen-Free CopperCDA: Alloy 102
101 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 101.0 % IACS at 68°F (20°C)248.2 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C10300 Oxygen-Free Extra Low Phosphorus (OFXLP) CopperOxygen-Free Extra Low PhosphorusDeoxidized Copper
UNS: C10300COMMERCIAL: Oxygen-Free Extra Low Phosphorus CopperCDA: Alloy 103
99 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 99.0 % IACS at 68°F (20°C)248.2 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C11000 ETP CopperElectrolytic Tough PitchPure Copper
UNS: C11000COMMERCIAL: Electrolytic Tough PitchCOMMERCIAL: ETP
101 % IACSTYPICAL · 20 °C · CDA Physical Properties section: Measured at 68°F (20°C), volume and weight basis206.8 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.025 in · 20 °C · Section Size: 0.025 in; Yield strength at 0.5% extension under load8.885–8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties section: Measured at 68°F (20°C). Footnote 1 specifies actual range 0.321 - 0.323 lb/cu in. (8.885 - 8.941 g/cm³)VERIFIED
Specs|
C12000 DLP CopperPhosphorus-Deoxidized Low Residual PhosphorusDeoxidized Copper
UNS: C12000COMMERCIAL: Deoxidized Low Phosphorus CopperCDA: Alloy 120
98 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 98.0 % IACS at 68°F (20°C)248.2 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C12200 DHP CopperPhosphorus-Deoxidized High Residual PhosphorusDeoxidized Copper
UNS: C12200COMMERCIAL: Deoxidized High Phosphorus CopperCDA: Alloy 122
85 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 85.0 % IACS at 68°F (20°C)206.8 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.25 · 20 °C · Section Size: 0.25; Section Size: 0.25 in; Yield strength at 0.5% extension under load8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C14500 Tellurium CopperTellurium CopperFree-Machining Copper
UNS: C14500COMMERCIAL: Tellurium CopperCDA: Alloy 145
93 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 93.0 % IACS at 68°F (20°C)275.8 MPaTYPICAL · 1/2 Hard (H02) · Rod · 1 · 20 °C · Section Size: 1; Cold Work: 20%; Section Size: 1 in; Yield strength at 0.5% extension under load8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C14700 Sulfur CopperSulfur CopperFree-Machining Copper
UNS: C14700COMMERCIAL: Sulfur CopperCDA: Alloy 147
95 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 95.0 % IACS at 68°F (20°C)268.9 MPaTYPICAL · 1/2 Hard (H02) · Rod · 2 · 20 °C · Section Size: 2; Section Size: 2 in; Yield strength at 0.5% extension under load8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C17200 Beryllium Copper (Alloy 25)Alloy 25Beryllium Copper
UNS: C17200COMMERCIAL: Beryllium Copper Alloy 25CDA: Alloy 172
22 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 22.0 % IACS at 68°F (20°C)1206.6 MPaTYPICAL · 1/2 Hard and Precipitation Heat Treated (TH02) · Flat Products · 0.188 · 20 °C · Section Size: 0.188; Section Size: 0.188 in; Yield strength at 0.5% extension under load8.027 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.29 lb/cu in. at 68°F (8.027 g/cm³ at 20°C)VERIFIED
Specs|
C17500 Beryllium Copper (Alloy 10)Alloy 10Beryllium Copper
UNS: C17500COMMERCIAL: Beryllium Copper Alloy 10CDA: Alloy 175
45 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 45.0 % IACS at 68°F (20°C)655 MPaTYPICAL · Hard and Precipitation Heat Treated (TH04) · Flat Products · 20 °C · Yield strength at 0.5% extension under load8.608 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.311 lb/cu in. at 68°F (8.608 g/cm³ at 20°C)VERIFIED
Specs|
C17510 Beryllium Copper (Alloy 3)Alloy 3Beryllium Copper
UNS: C17510COMMERCIAL: Beryllium Copper Alloy 3CDA: Alloy 175.1
48 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 48.0 % IACS at 68°F (20°C)744.6 MPaTYPICAL · 1/2 Hard and Precipitation Heat Treated (TH02) · Flat Products · 20 °C · Yield strength at 0.5% extension under load8.775 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.317 lb/cu in. at 68°F (8.775 g/cm³ at 20°C)VERIFIED
Specs|
C19400 High-Strength Modified Copper (HSM Copper)HSM CopperHigh-Performance Copper Alloys
UNS: C19400COMMERCIAL: High Strength Modified CopperCDA: Alloy 194
65 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 65.0 % IACS at 68°F (20°C)365.4 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.913 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.322 lb/cu in. at 68°F (8.913 g/cm³ at 20°C)VERIFIED
Specs|
C26000 Cartridge Brass 70/30Cartridge Brass 70/30Cartridge Brass
UNS: C26000COMMERCIAL: Cartridge BrassCDA: Alloy 260
28 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 28.0 % IACS at 68°F (20°C)275.8 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.525 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.308 lb/cu in. at 68°F (8.525 g/cm³ at 20°C)VERIFIED
Specs|
C26800 Yellow Brass 66%Yellow Brass 66%Yellow Brass
UNS: C26800COMMERCIAL: Yellow Brass 66%CDA: Alloy 268
27 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 27.0 % IACS at 68°F (20°C)344.7 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.47 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.306 lb/cu in. at 68°F (8.47 g/cm³ at 20°C)VERIFIED
Specs|
C27000 Yellow Brass 65%Yellow Brass 65%Yellow Brass
UNS: C27000COMMERCIAL: Yellow Brass 65%CDA: Alloy 270
27 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 27.0 % IACS at 68°F (20°C)344.7 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.47 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.306 lb/cu in. at 68°F (8.47 g/cm³ at 20°C)VERIFIED
Specs|
C27200 Yellow Brass 63%Yellow Brass 63%Yellow Brass
UNS: C27200COMMERCIAL: Yellow Brass 63%CDA: Alloy 272
27.6 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 27.6 % IACS at 68°F (20°C)379.2 MPaTYPICAL · Hard Drawn (H80) · Tube · 0.065 · 20 °C · Section Size: 0.065; Section Size: 0.065 in; Yield strength at 0.5% extension under load8.442 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.305 lb/cu in. at 68°F (8.442 g/cm³ at 20°C)VERIFIED
Specs|
C28000 Muntz Metal 60/40Muntz MetalYellow Brass
UNS: C28000COMMERCIAL: Muntz Metal 60/40CDA: Alloy 280
28 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 28.0 % IACS at 68°F (20°C)344.7 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.387 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.303 lb/cu in. at 68°F (8.387 g/cm³ at 20°C)VERIFIED
Specs|
C36000 Free-Cutting BrassFree-Cutting BrassFree-Machining Brass
UNS: C36000COMMERCIAL: Free-Cutting BrassCDA: Alloy 360
26 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 26.0 % IACS at 68°F (20°C)117.2 MPaTYPICAL · 1/2 Hard (H02) · Bar · 1.5 · 20 °C · Section Size: 1.5; Section Size: 1.5 in; Yield strength at 0.5% extension under load8.498 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.307 lb/cu in. at 68°F (8.498 g/cm³ at 20°C)VERIFIED
Specs|
C46400 Naval BrassNaval BrassNaval Brass
UNS: C46400COMMERCIAL: Naval BrassCDA: Alloy 464
26 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 26.0 % IACS at 68°F (20°C)172.4 MPaTYPICAL · As Hot Rolled (M20) · Flat Products · 1 · 20 °C · Section Size: 1; Section Size: 1 in; Yield strength at 0.5% extension under load8.415 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.304 lb/cu in. at 68°F (8.415 g/cm³ at 20°C)VERIFIED
Specs|
C51000 Phosphor Bronze 5% APhosphor Bronze 5% Grade APhosphor Bronze
UNS: C51000COMMERCIAL: Phosphor Bronze Grade ACDA: Alloy 510
15 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 15.0 % IACS at 68°F (20°C)372.3 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 20 °C · Yield strength at 0.5% extension under load8.858 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.32 lb/cu in. at 68°F (8.858 g/cm³ at 20°C)VERIFIED
Specs|
C52100 Phosphor Bronze 8% CPhosphor Bronze 8% Grade CPhosphor Bronze
UNS: C52100COMMERCIAL: Phosphor Bronze Grade CCDA: Alloy 521
13 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 13.0 % IACS at 68°F (20°C)441.3 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.802 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.318 lb/cu in. at 68°F (8.802 g/cm³ at 20°C)VERIFIED
Specs|
C54400 Free-Machining Phosphor Bronze (B-2)Phosphor Bronze B-2Phosphor Bronze
UNS: C54400COMMERCIAL: Free-Machining Phosphor BronzeCDA: Alloy 544
19 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 19.0 % IACS at 68°F (20°C)275.8 MPaTYPICAL · 1/2 Hard (H02) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.858 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.32 lb/cu in. at 68°F (8.858 g/cm³ at 20°C)VERIFIED
Specs|
C61400 Aluminum Bronze DAluminum Bronze DAluminum Bronze
UNS: C61400COMMERCIAL: Aluminum Bronze DCDA: Alloy 614
14 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 14.0 % IACS at 68°F (20°C)413.7 MPaTYPICAL · Hard (H04) · Flat Products · 0.125 · 20 °C · Section Size: 0.125; Section Size: 0.125 in; Yield strength at 0.5% extension under load7.889 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.285 lb/cu in. at 68°F (7.889 g/cm³ at 20°C)VERIFIED
Specs|
C63000 Nickel-Aluminum Bronze (AMS 4640)Nickel-Aluminum BronzeAluminum Bronze
UNS: C63000COMMERCIAL: Nickel-Aluminum Bronze (AMS 4640)CDA: Alloy 630
7 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 7.0 % IACS at 68°F (20°C)344.7 MPaTYPICAL · As Hot Extruded (M30) · Bar · 3 · 20 °C · Section Size: 3; Section Size: 3 in; Yield strength at 0.5% extension under load7.584 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.274 lb/cu in. at 68°F (7.584 g/cm³ at 20°C)VERIFIED
Specs|
C63200 Nickel-Aluminum Bronze (Naval Alloy)Naval Nickel-Aluminum BronzeAluminum Bronze
UNS: C63200COMMERCIAL: Nickel-Aluminum Bronze (Naval Alloy)CDA: Alloy 632
7 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 7.0 % IACS at 68°F (20°C)310.3 MPaTYPICAL · Light Anneal (O50) · Forgings · 5 · 20 °C · Section Size: 5; Section Size: 5 in; Yield strength at 0.5% extension under load7.64 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.276 lb/cu in. at 68°F (7.64 g/cm³ at 20°C)VERIFIED
Specs|
C65500 High-Silicon Bronze AHigh-Silicon Bronze ASilicon Bronze
UNS: C65500COMMERCIAL: High-Silicon Bronze ACDA: Alloy 655
7 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 7.0 % IACS at 68°F (20°C)241.3 MPaTYPICAL · 1/4 Hard (H01) · Flat Products · 0.04 · 20 °C · Section Size: 0.04; Section Size: 0.04 in; Yield strength at 0.5% extension under load8.525 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.308 lb/cu in. at 68°F (8.525 g/cm³ at 20°C)VERIFIED
Specs|
C70600 Copper-Nickel 90/10Copper-Nickel 90/10Copper-Nickel (Cupronickel)
UNS: C70600COMMERCIAL: 90/10 CupronickelCDA: Alloy 706
9 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 9.0 % IACS at 68°F (20°C)172.4 MPaTYPICAL · Hard (H04) · Bar · 20 °C · Yield strength at 0.5% extension under load8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C71500 Copper-Nickel 70/30Copper-Nickel 70/30Copper-Nickel (Cupronickel)
UNS: C71500COMMERCIAL: 70/30 CupronickelCDA: Alloy 715
4.6 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 4.6 % IACS at 68°F (20°C)—8.941 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.323 lb/cu in. at 68°F (8.941 g/cm³ at 20°C)VERIFIED
Specs|
C93200 Bearing Bronze (SAE 660)SAE 660Bearing Bronze
UNS: C93200COMMERCIAL: SAE 660 Bearing BronzeCDA: Alloy 932
12 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 12.0 % IACS at 68°F (20°C)96.5 MPaTYPICAL · As Centrifugal Cast (M02) · As Centrifugal Cast · 20 °C · Yield strength at 0.5% extension under load8.913 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.322 lb/cu in. at 68°F (8.913 g/cm³ at 20°C)VERIFIED
Specs|
C95400 Aluminum Bronze 9CAluminum Bronze 9CAluminum Bronze
UNS: C95400COMMERCIAL: Aluminum Bronze 9CCDA: Alloy 954
13 % IACSTYPICAL · 20 °C · CDA Physical Properties: Volume conductivity 13.0 % IACS at 68°F (20°C)206.8 MPaTYPICAL · As Centrifugal Cast (M02) · As Centrifugal Cast · 20 °C · Yield strength at 0.5% extension under load7.446 g/cm³TYPICAL · 20 °C · CDA Physical Properties: Density 0.269 lb/cu in. at 68°F (7.446 g/cm³ at 20°C)VERIFIED
Specs|
Chloroprene Rubber (CR / Neoprene)NeopreneOil & Fuel Resistant Elastomers
ASTM: CRISO: CRASTM-D2000: Type BC / BE
———VERIFIED
Specs|
EN-GJL-150 Gray Cast IronGG-15Gray Cast Iron
EN: EN-GJL-150W-Nr: EN-JL1020DIN: GG-15
——7.1 g/cm³TYPICALVERIFIED
Specs|
EN-GJL-200 Gray Cast IronGG-20Gray Cast Iron
EN: EN-GJL-200W-Nr: EN-JL1030DIN: GG-20
——7.15 g/cm³TYPICALVERIFIED
Specs|
EN-GJL-250 Gray Cast IronGG-25Gray Cast Iron
EN: EN-GJL-250W-Nr: EN-JL1040DIN: GG-25
——7.2 g/cm³TYPICALVERIFIED
Specs|
EN-GJL-300 Gray Cast IronGG-30Gray Cast Iron
EN: EN-GJL-300W-Nr: EN-JL1050DIN: GG-30
——7.25 g/cm³TYPICALVERIFIED
Specs|
EN-GJS-400-15 Ductile Cast IronEN-JS1030Ductile (Nodular) Iron
EN: EN-GJS-400-15W-Nr: EN-JS1030ISO: 1083/JS/400-15
—≥ 250 MPaMINIMUM · Ferritic7.1 g/cm³TYPICALVERIFIED
Specs|
EN-GJS-400-18 Ductile Cast IronGGG-40Ductile (Nodular) Iron
EN: EN-GJS-400-18W-Nr: EN-JS1020DIN: GGG-40
—≥ 250 MPaMINIMUM · Ferritic · Governing minimum 0.2% proof stress (Rp0.2) per EN 1563.7.1 g/cm³TYPICALVERIFIED
Specs|
EN-GJS-500-7 Ductile Cast IronGGG-50Ductile (Nodular) Iron
EN: EN-GJS-500-7W-Nr: EN-JS1050DIN: GGG-50
—≥ 320 MPaMINIMUM · Ferritic-Pearlitic · Governing minimum 0.2% proof stress (Rp0.2) per EN 1563.7.15 g/cm³TYPICALVERIFIED
Specs|
EN-GJS-600-3 Ductile Cast IronGGG-60Ductile (Nodular) Iron
EN: EN-GJS-600-3W-Nr: EN-JS1060DIN: GGG-60
—≥ 370 MPaMINIMUM · Pearlitic-Ferritic · Governing minimum 0.2% proof stress (Rp0.2) per EN 1563.7.15 g/cm³TYPICALVERIFIED
Specs|
EN-GJS-700-2 Ductile Cast IronGGG-70Ductile (Nodular) Iron
EN: EN-GJS-700-2W-Nr: EN-JS1070DIN: GGG-70
—≥ 420 MPaMINIMUM · Pearlitic · Governing minimum 0.2% proof stress (Rp0.2) per EN 1563.7.15 g/cm³TYPICALVERIFIED
Specs|
Ethylene Propylene Diene Rubber (EPDM)EPDMWeathering & Chemical Resistant Elastomers
ASTM: EPDMISO: EPDMASTM-D2000: Type BA / CA
———VERIFIED
Specs|
Fine Silver 999999 SilverFine Silver
UNS: P07010ISO: Ag99.9ASTM: Grade 99.90
106 % IACSTYPICAL · 20 °C≥ 40 MPaTYPICAL · Annealed (Soft) · Strip, Sheet, Wire, Bar10.49 g/cm³TYPICAL · 20 °CVERIFIED
Specs|
Fluoroelastomer (FKM)Viton® (Registered Trademark of Chemours)High-Temperature & Specialty Elastomers
ASTM: FKMISO: FPMASTM-D2000: Type HK
———VERIFIED
Specs|
Hydrogenated Nitrile Rubber (HNBR)Highly Saturated NitrileOil & Fuel Resistant Elastomers
ASTM: HNBRISO: HNBRASTM-D2000: Type DH
——1 g/cm³TYPICAL · Standard Peroxide-Cured 70 Shore A Compound (Fully Hydrogenated) · Unpigmented raw hydrogenated polymer base density.VERIFIED
Specs|
Natural Rubber (NR)Polyisoprene RubberGeneral-Purpose Diene Rubbers
ASTM: NRISO: NRASTM-D2000: Type AA
———VERIFIED
Specs|
Nitrile Butadiene Rubber (NBR)Buna-NOil & Fuel Resistant Elastomers
ASTM: NBRISO: NBRASTM-D2000: Type BF / BG / CH
———VERIFIED
Specs|
Polyester Polyurethane (AU)Polyester UrethanePolyurethane Elastomers
ASTM: AUISO: AUASTM-D2000: Type BG (AU)
———VERIFIED
Specs|
Polyether Polyurethane (EU)Polyether UrethanePolyurethane Elastomers
ASTM: EUISO: EUASTM-D2000: Type BG (EU)
———VERIFIED
Specs|
SAE 1006 Carbon SteelCarbon Steel
SAE: 1006AISI: 1006UNS: G10060
—≥ 280 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1008 Carbon SteelCarbon Steel
SAE: 1008AISI: 1008SPECIFICATION: SAE 1008 Carbon Steel Engineering Datasheet
—≥ 168.9 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1010 Carbon SteelCarbon Steel
SAE: 1010AISI: 1010SPECIFICATION: SAE 1010 Carbon Steel Engineering Datasheet
—≥ 179.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1012 Carbon SteelCarbon Steel
SAE: 1012AISI: 1012UNS: G10120
—≥ 315 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1015 Carbon SteelCarbon Steel
SAE: 1015AISI: 1015UNS: G10150
—≥ 325 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1016 Carbon SteelCarbon Steel
SAE: 1016AISI: 1016UNS: G10160
—≥ 350 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1017 Carbon SteelCarbon Steel
SAE: 1017AISI: 1017UNS: G10170
—≥ 365 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1018 Carbon SteelCarbon Steel
SAE: 1018AISI: 1018SPECIFICATION: SAE 1018 Carbon Steel Engineering Datasheet
—≥ 220.6 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1020 Carbon SteelCarbon Steel
SAE: 1020AISI: 1020SPECIFICATION: SAE 1020 Carbon Steel Engineering Datasheet
—≥ 206.8 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1021 Carbon SteelCarbon Steel
SAE: 1021AISI: 1021UNS: G10210
—≥ 400 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1022 Carbon SteelCarbon Steel
SAE: 1022AISI: 1022UNS: G10220
—≥ 405 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1025 Carbon SteelCarbon Steel
SAE: 1025AISI: 1025SPECIFICATION: SAE 1025 Carbon Steel Engineering Datasheet
—≥ 220.6 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.86 g/cm³TYPICALVERIFIED
Specs|
SAE 1026 Carbon SteelCarbon Steel
SAE: 1026AISI: 1026UNS: G10260
—≥ 435 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1030 Carbon SteelCarbon Steel
SAE: 1030AISI: 1030SPECIFICATION: SAE 1030 Carbon Steel Engineering Datasheet
—≥ 258.6 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1035 Carbon SteelCarbon Steel
SAE: 1035AISI: 1035SPECIFICATION: SAE 1035 Carbon Steel Engineering Datasheet
—≥ 272.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1038 Carbon SteelCarbon Steel
SAE: 1038AISI: 1038UNS: G10380
—≥ 495 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1040 Carbon SteelCarbon Steel
SAE: 1040AISI: 1040SPECIFICATION: SAE 1040 Carbon Steel Engineering Datasheet
—≥ 289.6 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1042 Carbon SteelCarbon Steel
SAE: 1042AISI: 1042UNS: G10420
—≥ 510 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1044 Carbon SteelCarbon Steel
SAE: 1044AISI: 1044UNS: G10440
—≥ 515 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1045 Carbon SteelCarbon Steel
SAE: 1045AISI: 1045SPECIFICATION: SAE 1045 Carbon Steel Engineering Datasheet
—≥ 310.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1050 Carbon SteelCarbon Steel
SAE: 1050AISI: 1050SPECIFICATION: SAE 1050 Carbon Steel Engineering Datasheet
—≥ 341.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1055 Carbon SteelCarbon Steel
SAE: 1055AISI: 1055UNS: G10550
—≥ 570 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1060 Carbon SteelCarbon Steel
SAE: 1060AISI: 1060SPECIFICATION: SAE 1060 Carbon Steel Engineering Datasheet
—≥ 372.3 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1065 Carbon SteelCarbon Steel
SAE: 1065AISI: 1065UNS: G10650
—≥ 600 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1070 Carbon SteelCarbon Steel
SAE: 1070AISI: 1070SPECIFICATION: SAE 1070 Carbon Steel Engineering Datasheet
—≥ 386.1 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1075 Carbon SteelCarbon Steel
SAE: 1075AISI: 1075UNS: G10750
—≥ 635 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1080 Carbon SteelCarbon Steel
SAE: 1080AISI: 1080SPECIFICATION: SAE 1080 Carbon Steel Engineering Datasheet
—≥ 424 MPaMINIMUM · Hot rolled (estimated minimum) · Bar · Producer estimated minimum, not a certified or guaranteed specification limit. Section size and test temperature are not stated.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1084 Carbon SteelCarbon Steel
SAE: 1084AISI: 1084UNS: G10840
—≥ 660 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1090 Carbon SteelCarbon Steel
SAE: 1090AISI: 1090UNS: G10900
—≥ 675 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1095 Carbon SteelCarbon Steel
SAE: 1095SPECIFICATION: SAE 1095 Carbon Steel Engineering Datasheet
—≥ 380 MPaMINIMUM · Spheroidize Annealed Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1117 Carbon SteelCarbon Steel
SAE: 1117AISI: 1117UNS: G11170
—≥ 395 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 1141 Carbon SteelCarbon Steel
SAE: 1141AISI: 1141UNS: G11410
—≥ 560 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1144 Carbon SteelCarbon Steel
SAE: 1144AISI: 1144UNS: G11440
—≥ 570 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 1215 Carbon SteelCarbon Steel
SAE: 1215AISI: 1215UNS: G12150
—≥ 415 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 12L14 Free-Machining SteelCarbon Steel
SAE: 12L14AISI: 12L14UNS: G12144
—≥ 415 MPaMINIMUM · Cold Drawn Bar (19 to 32 mm) · Bar7.87 g/cm³TYPICALVERIFIED
Specs|
SAE 4118 Alloy SteelAlloy Steel
SAE: 4118AISI: 4118UNS: G41180
—≥ 380 MPaMINIMUM · Normalized Bar (25 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4130 Alloy SteelAlloy Steel
SAE: 4130SPECIFICATION: SAE 4130 Alloy Steel Engineering Datasheet
—≥ 435 MPaMINIMUM · Normalized Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4137 Alloy SteelAlloy Steel
SAE: 4137AISI: 4137UNS: G41370
—≥ 440 MPaMINIMUM · Normalized Bar (25 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4140 Alloy SteelAlloy Steel
SAE: 4140AISI: 4140SPECIFICATION: SAE 4140 Alloy Steel Engineering Datasheet
—≥ 740 MPaMINIMUM · Quenched and tempered (voestalpine supply) · Bar · 10–100 mm · voestalpine supply properties for the stated section range; source does not specify test temperature. Not extrapolated to other products or heat treatments.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4142 Alloy SteelAlloy Steel
SAE: 4142SPECIFICATION: SAE 4142 Alloy Steel Engineering Datasheet
—≥ 640 MPaMINIMUM · Normalized Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4145 Alloy SteelAlloy Steel
SAE: 4145AISI: 4145UNS: G41450
—≥ 470 MPaMINIMUM · Normalized Bar (25 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4150 Alloy SteelAlloy Steel
SAE: 4150SPECIFICATION: SAE 4150 Alloy Steel Engineering Datasheet
—≥ 430 MPaMINIMUM · Annealed Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4320 Alloy SteelAlloy Steel
SAE: 4320AISI: 4320UNS: G43200
—≥ 420 MPaMINIMUM · Normalized Bar (25 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4340 Alloy SteelAlloy Steel
SAE: 4340SPECIFICATION: SAE 4340 Alloy Steel Engineering Datasheet
—≥ 470 MPaMINIMUM · Annealed Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 4620 Alloy SteelAlloy Steel
SAE: 4620SPECIFICATION: SAE 4620 Alloy Steel Engineering Datasheet
—≥ 360 MPaMINIMUM · Normalized Bar - Core Properties · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 5120 Alloy SteelAlloy Steel
SAE: 5120SPECIFICATION: SAE 5120 Alloy Steel Engineering Datasheet
—≥ 340 MPaMINIMUM · Normalized Bar - Core Properties · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 5140 Alloy SteelAlloy Steel
SAE: 5140SPECIFICATION: SAE 5140 Alloy Steel Engineering Datasheet
—≥ 410 MPaMINIMUM · Annealed Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 5160 Alloy SteelAlloy Steel
SAE: 5160SPECIFICATION: SAE 5160 Alloy Steel Engineering Datasheet
—≥ 400 MPaMINIMUM · Annealed Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 52100 Alloy SteelAlloy Steel
SAE: 52100SPECIFICATION: SAE 52100 Alloy Steel Engineering Datasheet
—≥ 380 MPaMINIMUM · Spheroidize Annealed Bar · Bar7.81 g/cm³TYPICALVERIFIED
Specs|
SAE 6150 Alloy SteelAlloy Steel
SAE: 6150SPECIFICATION: SAE 6150 Alloy Steel Engineering Datasheet
—≥ 410 MPaMINIMUM · Annealed Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 8617 Alloy SteelAlloy Steel
SAE: 8617AISI: 8617UNS: G86170
—≥ 360 MPaMINIMUM · Normalized Bar (25 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 8620 Alloy SteelAlloy Steel
SAE: 8620SPECIFICATION: SAE 8620 Alloy Steel Engineering Datasheet
—≥ 380 MPaMINIMUM · Normalized Bar (870°C) - Core Properties · Bar · Core mechanical properties.7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 8622 Alloy SteelAlloy Steel
SAE: 8622AISI: 8622UNS: G86220
—≥ 390 MPaMINIMUM · Normalized Bar (25 mm) · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 8630 Alloy SteelAlloy Steel
SAE: 8630SPECIFICATION: SAE 8630 Alloy Steel Engineering Datasheet
—≥ 450 MPaMINIMUM · Normalized Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 8640 Alloy SteelAlloy Steel
SAE: 8640SPECIFICATION: SAE 8640 Alloy Steel Engineering Datasheet
—≥ 415 MPaMINIMUM · Annealed Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 8740 Alloy SteelAlloy Steel
SAE: 8740SPECIFICATION: SAE 8740 Alloy Steel Engineering Datasheet
—≥ 415 MPaMINIMUM · Annealed Bar · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
SAE 9310 Alloy SteelAlloy Steel
SAE: 9310SPECIFICATION: SAE 9310 Alloy Steel Engineering Datasheet
—≥ 585 MPaMINIMUM · Normalized Bar - Core Properties · Bar7.85 g/cm³TYPICALVERIFIED
Specs|
Silicone Rubber (VMQ)SiliconeHigh-Temperature & Specialty Elastomers
ASTM: VMQISO: VMQASTM-D2000: Type FC / FE / GE
———VERIFIED
Specs|
Silver 800800 SilverAlloyed Silver
DIN: 2.3800ISO: Ag800EN: AgCu20
68 % IACSTYPICAL · 20 °C≥ 200 MPaTYPICAL · Annealed (Soft) · Strip & Wire10.15 g/cm³TYPICAL · 20 °CVERIFIED
Specs|
Silver 835835 SilverAlloyed Silver
DIN: 2.3835ISO: Ag835EN: AgCu16.5
72 % IACSTYPICAL · 20 °C≥ 180 MPaTYPICAL · Annealed (Soft) · Strip & Wire10.22 g/cm³TYPICAL · 20 °CVERIFIED
Specs|
Silver 900900 SilverAlloyed Silver
UNS: P07900ISO: Ag900US-COIN: Coin Silver 900
78 % IACSTYPICAL · 20 °C≥ 150 MPaTYPICAL · Annealed (Soft) · Strip & Wire10.31 g/cm³TYPICAL · 20 °CVERIFIED
Specs|
Silver 950950 SilverAlloyed Silver
ISO: Ag950DIN: Ag950FR-MINERVE: 1st Standard (950)
90 % IACSTYPICAL · 20 °C≥ 95 MPaTYPICAL · Annealed (Soft) · Strip & Wire10.38 g/cm³TYPICAL · 20 °CVERIFIED
Specs|
Silver 970970 SilverAlloyed Silver
ISO: Ag970DIN: Ag970EN: AgCu3
96 % IACSTYPICAL · 20 °C≥ 65 MPaTYPICAL · Annealed (Soft) · Strip & Wire10.43 g/cm³TYPICAL · 20 °CVERIFIED
Specs|
Sterling Silver 925Sterling SilverSterling Silver
UNS: P07925ISO: Ag925ASTM: B742 Grade 92.5
84 % IACSTYPICAL · 20 °C≥ 125 MPaTYPICAL · Annealed (O Temper) · Strip, Sheet, Wire10.36 g/cm³TYPICAL · 20 °CVERIFIED
Specs|
Styrene-Butadiene Rubber (SBR)Buna-SGeneral-Purpose Diene Rubbers
ASTM: SBRISO: SBRASTM-D2000: Type AA / BA
———VERIFIED
Specs|
Type 416 Stainless SteelMartensitic
UNS: S41600
——7.64 g/cm³TYPICAL · Producer physical property; test temperature and product condition not stated.VERIFIED
Specs|